> Question:
> How does osage orange compare to hickory for handles?
> I've been fooling around with shaving the necks of certain hammer
> handles way down. Just as they get really comfy to wield, the darn
> handle breaks.
> Would osage tolerate more thinning than hickory?...pf

Osage orange is the wood of choice for archery bows, therefore would bend 
but not break while thin.YMMV 