[TheForge] Charcoal
Rich Maynard
rich at maynard.org.uk
Wed Sep 17 04:06:28 EDT 2008
As far as I can see (if you can get hold of it at a decent price) the main
downside is it's lack of calorific value; you'll get through it a lot
quicker. The smiths I've seen using it seem to have a routine of putting
their steel back into the fire and putting on another handful of charcoal
each time.
Rich M.
Richard Maynard - Artist Blacksmith
The Forge, Much Hadham, Hertfordshire SG10 6BS
The Forge Experience - be a blacksmith for a day!
http://www.muchhadhamforge.co.uk/experience.pdf
rich at muchhadhamforge.co.uk
www.muchhadhamforge.co.uk
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Brian Reedy
Sent: 17 September 2008 06:26
To: The Forge
Subject: [TheForge] Charcoal
Thanks for all the positive feedback regarding the discussion of coal,
charcoal or propane. Because of all the suggestions from members I'm
switching to charcoal for the following reasons: accessibility to quality
fuel, lack of noxious smoke, and one comment from an ABANA member made the
most impact by far...not having to "constantly be dicking with the fire".
It seems that charcoal has nearly every property that coal lacks. Cleaner
burning, readily available, less problems with forge welding......granted
there's poppers and flyers from the fire occasionally. Now, someone talk me
out of using charcoal and convince me to use something else. Again, thanks
for the feedback. It's great to hear from blacksmiths in residential
areas!!!!
Brian Reedy __________________________________________________________
A well regulated militia being necessary to the security of a free State,
the right of the People to keep and bear arms shall not be infringed.
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list