I find it rust resistant. Spraying clear over it will help.  Option: sell 
them a maintenance contract.



> Hello
> Frequently I will finish an item brushing it with a brass brush for a
> color, decorative effect.  As I have not used this on an outdoor item
> .is this finish a rust proofing finish?
> 