That should work. The trickiest part may be welding the steel to the anvil top, if the anvil top is wrought iron. You may need a high nickel rod for that connection. There are some welding experts on this list who may chime in.
Aubrey
________________________________________
From: theforge-bounces at mailman.qth.net [theforge-bounces at mailman.qth.net] On Behalf Of Jonathan Barnhart [blakkpawss at yahoo.com]
Sent: Wednesday, September 10, 2008 2:04 PM
To: The Forge
Subject: RE: [TheForge] Top of a broken anvil
Well, I'm planning on using some 2" think steel in a flat rectangular form to make pieces to go under it. I'd planned on setting them side by side and orienting them vertically. I figured that they'd be strongest against the force of the hammer blow in this configuraion. Will it be safe then to make one large flat plate added under these in a horizontal manner as a mount plate? I figured on setting a larger rectangle under with some holes drilled in it. Then when I make my base for the anvil, I'll set some allthread in the base to match the holes. Then, I can tighten it down with some nuts.
--- On Wed, 9/10/08, Washington, Aubrey O. <awashington at ou.edu> wrote:
> From: Washington, Aubrey O. <awashington at ou.edu>
> Subject: RE: [TheForge] Top of a broken anvil
> To: "blakkpawss at yahoo.com" <blakkpawss at yahoo.com>, "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
> Date: Wednesday, September 10, 2008, 1:49 PM
> One point that may have been lost in the discussion is the
> orientation of steel plates. If you are going to laminate
> several plates together, orient them vertically rather than
> horizontally.
>
> Aubrey
>
> -----------------------------------------------------------------------
> [snip]
>
> So, in conclusion I think that steel and welding is the way
> to go. I'll be working out the final details of the
> project. So, if anyone can think of anything that
> hasn't been mentioned yet or a better way of doing
> something that I'm about to do, please speak up. When
> I'm(we're) done fixing it, I'll send out some
> pics.
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list