Watch the line wrap.

They make sheets of mica pieces and resin. You can slump it into your 
metal fixture in a kitchen oven.

Steve

Grant Marcoux wrote:
> Bob, et al:  there is a product that simulates mica that is used by shade
> makers, which is a glass-impregnated resin that bends to shape and has the
> look of natural material.  I don't remember the name, but you might search
> under "simulated mica" or something.  Grant
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net]On Behalf Of Peter Fels &
> Phoebe Palmer
> Sent: Sunday, October 12, 2008 11:22 PM
> To: Blacksmithing List Sponsored by ABANA
> Subject: Re: [TheForge] Wall Sconce Shade Material
>
>
> Mica or isinglass has been used for that function for a very long time
> Bob...pf
>
> Bob Smolen wrote:
>   
>> There was a picture of a nice wall sconce (lamp) in an old Anvil's Ring.
>> What is a good material to use for the shade that will allow light to
>> radiate yet not be flammable if the bulb is on for a long time? I suppose
>>     
> a
>   
>> thin metal would work if the goal was to allow light to radiate from the
>>     
> top
>   
>> and bottom. Is there a good material that is also somewhat translucent yet
>> safe?
>> Thanks,
>> Bob
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>
>>     
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
> No virus found in this incoming message.
> Checked by AVG.
> Version: 7.5.524 / Virus Database: 270.8.0/1721 - Release Date: 10/12/2008
> 12:00 PM
>
> No virus found in this outgoing message.
> Checked by AVG.
> Version: 7.5.524 / Virus Database: 270.8.0/1722 - Release Date: 10/13/2008
> 7:50 AM
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>
>   


More information about the TheForge mailing list