[TheForge] Evaporust
Jerry Frost
akfrosty at mtaonline.net
Sat May 31 00:48:37 EDT 2008
Phosphoric acid is the rust converter in Ospho, same as
Naval Jelly. Good stuff.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
From: "robert hensarling" <rhrocker at hilconet.com>
> Peter, could that possibly be the same stuff as
> Ospho? Usually comes in a one gallon plastic bottle,
> bluish in color. It's one of the acids, maybe
> diluted hydrochloric? I'm not sure. If you have
> something that's really rusty, this stuff attacks the
> rust making it inert, turning it both black, and sort
> of a white powder. It's a primer also. Good stuff,
> just have to use the usual cautions. However, this
> may not be what you're looking for.