Peter, could that possibly be the same stuff as Ospho? Usually comes in a
one gallon plastic bottle, bluish in color. It's one of the acids, maybe
diluted hydrochloric? I'm not sure. If you have something that's really
rusty, this stuff attacks the rust making it inert, turning it both black,
and sort of a white powder. It's a primer also. Good stuff, just have to
use the usual cautions. However, this may not be what you're looking for.
----- Original Message -----
From: "Peter Hirst" <saltydog335 at aol.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, May 30, 2008 6:02 PM
Subject: [TheForge] Evaporust
have been trying to get get Evaporust: maybe the worst distribution sytem
for any product I have ever encountered. The so- called distributor in
Connecticut currently stocks exactly one five-gallon pail, which may or may
not still be there if I make the trip, and can't tell me if or where its
retailed. Neither can the Mfr. Only refers me back to the CT distributor. I
understand that for squeaky clean rust removal, its the stuff to use: anyone
know where I can get it in New England? Or if there is another chelating
agent available that is a decent substitute?
thanks
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list