So what is the ht temp of Al? Yes, be careful with heat on aluminum. A friend had a baked-on fancy paint job on a scuba tank done at a body shop. The heat lamp was apparently hot enough to alter the structural integrity of the metal and it exploded during the filling process. It caused serious bodily injury. Ron C