concur!
Even if for practice. What do you have when you get through?
You STILL can't beat on it.


----- Original Message ----- 
From: "Andrew Vida" <osan at netlabs.net>
To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, May 21, 2008 2:37 PM
Subject: Re: [TheForge] Re: Welding cast iron


>
>
> Peter Fels & Phoebe Palmer wrote:
>> A related approach is to cast a screw in graphite compound or refractory 
>> and build up a nut with brazing...chip out the screw core after it cools.
>> Want another dozen impractical solutions?...pf
>
> Unless the vise is one of those $1000 Starrett machinist numbers, it would 
> seem a waste to put so much effort into repairing a third-rate vise.
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
> 



More information about the TheForge mailing list