Made a few things from them over the years and thought they were about that 
grade. Thanks for the info
L Brown

At 11:19 PM 5/13/2008 -0500, you wrote:
>I just came back from doing some work at Arvin Meritor in Hopkinsville, 
>KY. I found out they make tie rods for many automakers and that they make 
>all the tie rods from 5160 steel... humm.. sounds like a new source for 
>known metal.
>
>
>mike
>
>
>--