[TheForge] Re: File Making, sniffing up wrought iron

Andrew Vida osan at netlabs.net
Wed Mar 26 19:55:01 EST 2008



Graham Whaley wrote:

>  I'd like some wrought just to play with, and keep my eyes open for some
> just 'lying around'.  So far no luck. 

	Go to old industrial sites, especially those on the water.  Abandoned 
and demolished sites are best.  Old shipyards, ship graveyards are very 
good sources.  England should have large amounts of wrought rotting in 
the various waters.  Once you develop an eye for wrought, you will 
notice it in many places.  I find wrought iron all over the place, which 
makes sense given the umpteen millions of tons that were produced.


More information about the TheForge mailing list