Speaking of fumes, much of the wrought iron I pulled out of Raritan Bay
in Perth Amboy gives off a fume that is really nasty. You get the
tiniest whiff and everything inside you says "NO!". I have learned to
steer clear of this. Put the iron in the fire awhile and let whatever
noxious things that are there burn off while giving a respectful berth.
What I could not quite figure is what those noxious things may have
been. The fumes are most acrid - very harsh on the nose, and something
of a singular sensation (please, no lapsing into "A Chorus Line"). I
also notice the occasional strange blue flame. Not like copper, but not
like anything else either, of which I am familiar. Any ideas? This
iron has lain in the brackish-to-salty waters of the bay for at least 50
years, closer to 100 in most cases I would imagine - old ship graveyard.
-Andy
Larry Brown wrote:
> Thanks for the information in the post, I always try to stay away from
> the fumes as it stinks, but the cyanide information is really good to be
> aware of. Don't use it much, got the can 2nd hand and have had it 20+ yrs.
> Larry Brown