[TheForge] Setting Railing Posts
Woolley
wjec at comcast.net
Fri Mar 14 21:09:00 EST 2008
George,
Thanks for the response. Good info on finishing the pour, I will
certainly keep that in mind since you are not the only person who gave
me that advice.( Larry Brown) Anyway, I usually double the diameter of
the post for the hole width to give me some play, so it is encouraging
to hear you do the same. I use Rockit, it works well for me. Union
ironworkers, seen plenty up close in action, non better. Mostly
Philadelphia Local 401.
Best,
Bill Woolley
G. Watts wrote:
> Bill,
> 4" embedment seems pretty typical for the 1 1/2" rail that we do quite
> often, though I've had to go as deep as 12" on a school job where the rail
> sat on a 6" curb and the engineer wanted the stress down in the beef of the
> slab. Usually go with 3" holes so that there's some room for adjustment
> (also works for larger doubled plate with a gap between posts like a tuning
> fork shape). I use whatever the fabricator supplies...Rockit, Pour-Rock,
> etc. Given the choice, I like to leave the Pour-Rock 1/2-3/4" low and
> finish slightly crowned with a fairly dry topping mix, packed in tightly-
> seems to resist weathering better than the pourable stuff and matches the
> native concrete color better as well.
>
> George.
>
>
> Union Ironworker
> Local 229, San Diego
> Metro Iron Works
>
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net]On Behalf Of Woolley
> Sent: Thursday, March 13, 2008 6:57 AM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] Setting Railing Posts
>
>
> Reposting this, anybody?
>
>
>
> Woolley wrote:
>
>> Greetings,
>>
>> For anyone setting railings in concrete, brick, stone etc., how deep
>> are you setting your railing posts? I have been setting mine 4" deep
>> but I was just wondering what others were doing. I use hydraulic
>> cement, a 2" core drill for 1" posts, but have recently considered
>> buying a carbide tipped 1 1/2" for this. What are you guys using?
>>
>> Regards,
>> Bill Woolley
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
More information about the TheForge
mailing list