Mcmaster-Carr part # 4179A924
Bimetal Band Saw Blade 9'4" Length, 1/2" W, .025" Thk, 10-14 Tpi, Vari/
Vari
In stock at $33.19 Each
On Mar 5, 2008, at 4:25 PM, PlumDon at aol.com wrote:
> Looking for a couple of somewhat odd-sized blades (112") for my old
> (but
> great) 16" Walker Turner bandsaw. Prefer the best quality 1/2" bi-
> metal. Haven't
> bought any for a couple years and last supplier appears to be gone.
> Any
> recommendations re a good source for custom blades much appreciated.
> I definitely
> do not want to weld up my own.
>
> Thanks for any suggestions
>
> Don Plummer
>
>
>
> **************It's Tax Time! Get tips, forms, and advice on AOL
> Money &
> Finance. (http://money.aol.com/tax?NCID=aolprf00030000000001)
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
James Binnion
jbin at well.com
More information about the TheForge
mailing list