Burgon indeed wins the prize.  Even though they don't list it on thir site, 
they got right back to me with a quote on 1045 in the relativley small 
quantity I need.  I am sending my order today.  Thanks for the help, all

Keziah




----- Original Message ----- 
From: "Phil" <mobjak at yahoo.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, March 04, 2008 7:35 AM
Subject: Re: [TheForge] 1045 Steel (?)


Peter:

I've used the following folks in New Hampshire.
Additionally, McMaster Carr carries 1045.

Phil

Name: Burgon Tool Steel
Address: 20 Durham Street
Address2: Pease International Tradeport
City: Portsmouth
State: NH
Zip: 3801
Zipplus:
Country:
Postalcode:
Phone: 800-258-7106
Phone2: 603-430-9200
Fax: 603-430-4004
Email: sales at burgon.com
Website: www.burgon.com
--- Peter Hirst <saltydog335 at aol.com> wrote:

> I am having a terrible time locating a supply of
> 1045 steel (or equivalent) in eastern Massachusetts.
>  Doesn't seem like it should be that tough an order,
> but my two old reliable sources were no help.  The
> sales people didn't even know what I was talking
> about, much less where to refer me.  1018 cold drawn
> was the nearest they could come up with, and that
> aint gonna cut it.  I am making  garden tools (I
> have done the prototypes in 1018), like the ones
> that were made near here by Snow & Neally until a
> couple of years ago.  They are easy designs, and
> just require material a little tougher than mild
> steel, and after a little research I have determined
> that 1045 is just about the stuff I want.  I can buy
> a shipload of it from Earle M Jorgensen, but so far
> I havent found anyplace I can get a hundred feet or
> so (of 3/8 round).  AM I asking for the wrong stuff?
>  SHould I be looking at something else?  ANy Ideas?
> Thanks.
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>



      ____________________________________________________________________________________
Never miss a thing.  Make Yahoo your home page.
http://www.yahoo.com/r/hs
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________




More information about the TheForge mailing list