[TheForge] Steel attaching to masonry
Jerry Frost
akfrosty at mtaonline.net
Sun Mar 2 01:53:33 EST 2008
You see them mortared into joints all the time and they
seem to hold up fine. I'd make the anchor pretty long
but wouldn't worry about it over much.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
From: "Mark Novak" <mark at fireworkspdx.com>
>
> If so, I may have not communicated clearly. My
> concern is less with the hinges themselves than with
> how the hinge is mounted into the masonry. Is there
> a material that will expand and contract with the
> steel, so that the hinges and doors don't tear away
> from cracking masonry? Is it merely a matter of
> leaving enough distance between where the hinges
> connect to masonry and the opening of the fireplace,
> or am I going to have to build a frame and a floor
> support that the doors can swing on, so that they
> aren't connected to the masonry at all?
>
> Thanks for your help,
> Mark