Loose hinges on doors that do not press against each other.
Then let them expand. The motion doesn't count.
Mike Graf
Mark Novak wrote:
> I'm planning on building a stone and masonry outdoor oven and
> fireplace with insulated steel doors, but I'm concerned about the
> doors getting hot and, upon swelling and contracting, cracking the
> masonry. Any advice on how to mount the doors to the masonry?
>
> Thanks,