[TheForge] coal or charcoal morph to Evaporust
Peter Fels & Phoebe Palmer
artgawk at thegrid.net
Wed Jun 25 20:14:39 EDT 2008
Old Dr Tinkerpaw swore that coke was best at freeing up rusted parts.
It also makes a spiffy annodizing medium for titanium i'm told...pf
James Binnion wrote:
> I use Coke as a cleaner of stainless steel tumbling media to remove the
> smut that builds up from use. The carbonic acid (CO2 in water) and
> phosphoric acid are good, mild, metal cleaners.
>
>
> James Binnion
> jbin at well.com
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>