Why fart around with this at all? Go to the scrap yard and find a piece
of 6" solid round or 4" solid square and do the job correctly. If it
costs you $50, so what?
Just a thought anyway.
Peter Fels & Phoebe Palmer wrote:
> Lynn;
> You want as much solid mass as possible for your TH anvil.
> If you are going to laminate the elements, orient them vertically and
> weld the heck out of them.100% penetration if possible.
> Square tubing will waste a lot of your effort....just too light...pf
>
> Lynn and Susan Lang wrote:
>> Hello
>>
>> I am looking to build a treadle hammer. The anvil base is usually
>> constructed from laminated stock, would an anvil base constructed from
>> either 3 or 4" thick wall pipe or square tubing be structurally
>> equivalent or as functional?
>> Thank you
>> lynn
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
--
-Andy V.
no .sig
go .fig
More information about the TheForge
mailing list