Washington, Aubrey O. awashington at ou.edu
Mon Jun 2 12:01:20 EDT 2008


Really?!  Where can I find more details about how to do this.  (My arc welder is AC only.)

Aubrey

________________________________________
From: theforge-bounces at mailman.qth.net [theforge-bounces at mailman.qth.net] On Behalf Of Jerry Frost [akfrosty at mtaonline.net]
Sent: Saturday, May 31, 2008 10:04 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] tig

You can turn a MIG into a scratch start TIG by pulling
the wire and driving a tungsten into the mig tip. You
may have to drill the mig tip out so the tungsten will
fit but leave it tight.

Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks

Meadow Lakes, AK.


From: <schade at acegroup.cc>


>I think I remember reading here some time ago about a
>way to turn an arc welder into a scratch start TIG
>welder.
>
> Am I dreaming or is this doable? If it is can someone
> point me in the right direction?
>
> Thanks.
>
> Bob
>
>

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________


More information about the TheForge mailing list