[TheForge] Clear finish

Andrew Vida osan at netlabs.net
Mon Jul 21 15:22:08 EDT 2008



Andy Gladish wrote:
> Andy-
> I used a variation on this for our living room floor.
> Worked ok, but since then have replaced it with regular commercial wax. 
> Reason was, using enough turpentine to make the wax flow made our LR 
> unliveable for days.
> BTW, the floor was a lime/sand mix soaked in boiled linseed oil- very 
> nice and user friendly.

	How thick is the layer of lime/sand/oil?  Just wondering.  I wonder if 
this would be a superior embedding layer for radiant floor heating 
conduits.  Sets up pretty hard but not like concrete.  Digging up a 
section would be easier (?)