[TheForge] Clear finish
Peter Fels & Phoebe Palmer
artgawk at thegrid.net
Sat Jul 19 21:29:00 EDT 2008
Master Chase said to apply it just short of smoking hot and wipe off the
excess later.....this is an interior finish....pf
James Binnion wrote:
> Johnsons paste wax, easy to apply , easy for customer to maintain,
> simple to repair, doesn't crack or peel
>
> On Jul 19, 2008, at 1:45 PM, Andy Gladish wrote:
>
>> This is kind of an old topic, but I'm doing three fairly modern
>> looking barstools that will be used indoors, the customer has asked
>> for a clear finish.
>> Anyone want to share their favorite potions? I don't think the
>> blackened finishes are right for this project, and it's too small an
>> order to P-coat.
>> Thanks!
>> Andy
>> --
>> Andy Gladish, Metal Work
>> Element Forge
>> www.ElementFe.com
>> Email: andy at elementfe.com
>> Portfolio @ elementfe.carbonmade.com
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>
> James Binnion
> jbin at well.com
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list