I have had good luck using pf varying diameters, and cutting "gores" of
differing lengths to induce the taper.  These gores are cut on a taper the
length of the pipe and the pipes is then closed and welded.  Bark texture
has been done with torch and/or plasma cutter held at an angle.  I have an
example in my "sculpture" section on my website, with pictures of the Almond
Eagle. at www.grantsforge.com

These methods work

Grant

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of robert hensarling
Sent: Wednesday, July 02, 2008 11:01 AM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Stumped!


A blacksmith by the name of Joe Miller has done that before.  He talked
about it, and even demoed a little of it on a DVD that I got from Roger
Degner.  Miller is a fantastic artist.  He makes jigs and what not, to build
all of the various items he makes.  The DVD is very interesting.  It can be
bought for about $7, or I believe you can rent it.
Show the results when you've made one Bob.
----- Original Message -----
From: "Bob Willman" <blcksmth at wcnet.org>
To: <mlforge at cebridge.net>; "'Blacksmithing List Sponsored by ABANA'"
<theforge at mailman.qth.net>
Sent: Wednesday, July 02, 2008 10:44 AM
Subject: RE: [TheForge] Stumped!


> Sheet metal rolled and shaped to look like roots. Weld beads to
> simulate bark.
>
>
> Bob Willman
> Bowling Green, Ohio
> The Eagle's Anvil
> WB8NQW
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of
> mlforge at cebridge.net
> Sent: Wednesday, July 02, 2008 5:17 AM
> To: theforge at mailman.qth.net
> Subject: [TheForge] Stumped!
>
> I'm trying to make a stump, but no seaming to work out. I started with a
> piece of 6  inch pipe and attached several tapered pieces of 5/8 round
> with
> bark texture. I'm  looking to get the look of roots and a wider base area.
> Anyone have any  suggustions. Thanks, Ralph      Maple Leaf Forge Ralph
> Neumeister     _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________

No virus found in this incoming message.
Checked by AVG.
Version: 7.5.524 / Virus Database: 270.4.4/1530 - Release Date: 7/2/2008
8:05 AM

No virus found in this outgoing message.
Checked by AVG.
Version: 7.5.524 / Virus Database: 270.4.4/1530 - Release Date: 7/2/2008
8:05 AM



More information about the TheForge mailing list