[TheForge] Torch, Propane

paul forge at wi.rr.com
Thu Jan 31 13:52:00 EST 2008


Ron Childers wrote:
> I've used the same acetylene regulator with propane for 15 years with no
> problems- a #3 propane tip for the big Smith for serious cutting and the
> small Victor as-is for localized heating, etc. Ron C

No problem with the regulator, but the concern is with the hose.
Here is one source to view.

http://www.weldingmag.com/323/Issue/Article/False/45963/Issue

I will admit to having broken this rule but that is a personal risk I 
chose to take, and doesn't make it a good practice.
bad plumber...


-- 
Paul Sperbeck
WB9HCO
jadap

  "The difference between genius and stupidity is that
genius has its limits." -Albert Einstein