Larry Brown wrote:
lot of old star drills were s series steels and are
quickly converted
to
slitting chisels etc and are real cheap at flea
markets as no one
remembers
what they are for. I have heard some great
descriptions
I second the question as to typical composition,
having also gotten a number of these at auction.
Are they one type of steel throughout so you could
cut off the star and re-use the shaft as punches?