[TheForge] Re: Free the Stake!

Larry Brown lp.brown at verizon.net
Mon Jan 21 10:44:06 EST 2008


Something I haven't seen suggested:
Cut the stake off close to the block. Reforge a taper on the stake. Drill a 
bunch of holes in the stub making as large a hole as possible or blow 
through with a torch. Heat the stub remains with a torch, preferably a 
large or rosebud tip. This will force the stub to upset into itself and 
will probably fall out or be easily driven out after cooling with the block 
upside down