[TheForge] Free the Stake!
Dan Brewer
danqualman at gmail.com
Sat Jan 19 14:57:08 EST 2008
negative is attached to the piece you want to have stuff removed from and
the Positive to the piece you want the stuff to be attached to.
Dan
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Peter Hirst
Sent: Saturday, January 19, 2008 11:42 AM
To: Sponsored by ABANA
Subject: Re: [TheForge] Free the Stake!
Uhh, the positive to which?
----- Original Message -----
From: "Dan Brewer" <danqualman at gmail.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Saturday, January 19, 2008 1:24 PM
Subject: RE: [TheForge] Free the Stake!
> All you are doing by putting something in the water is to make the water
> more conductive. So soda, salt, acid, all work. Attach the positive to
> the
> piece you want stuff to be removed from and the positive to the thing you
> want to have coated. All of this in a plastic bucket .
>
> Dan in Auburn
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of A Vida
> Sent: Saturday, January 19, 2008 6:04 AM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] Free the Stake!
>
> You can use ANYTHING as an electrolyte. Pee in the water if you
> want.
> It will work just fine.
>
> Dan Scheid wrote:
>> No keep them the same. The reason I like a mild HC is HC love to eat
>> rust.
>> But a soda is more environmentally friendly
>> Dan Scheid
>>
>> I've done a little electrolytic derusting lately, using an alkaline
> (washing
>>
>> soda) batheand putting the work piece on the cathode. I've never used an
>> acid medium, but I would assume it requires reversing the polarity, yes?
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list