[TheForge] fire screen
Grant Marcoux
gblacksmith at alamedanet.net
Thu Feb 28 23:39:43 EST 2008
Andy: I use a #10 mesh of either .025. .035 or .045 wire diameter.
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Andy Gladish
Sent: Thursday, February 28, 2008 6:56 AM
To: Sponsored by ABANA
Subject: [TheForge] fire screen
Could someone please recommend a wire size for the screen on a
freestanding fire screen?
I spent some time on McMaster's website but with 98948.9834 X 10^7 choices
it just gave me a headache...
Thanks!
Andy Gladish
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.5.516 / Virus Database: 269.21.1/1303 - Release Date: 2/28/2008
12:14 PM
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.5.516 / Virus Database: 269.21.1/1303 - Release Date: 2/28/2008
12:14 PM
More information about the TheForge
mailing list