[TheForge] Removing Zinc and Cadium

Peter Hirst saltydog335 at aol.com
Sat Feb 23 12:34:48 EST 2008


So one would conclude that elemental zinc is not a big risk, even in 
solution.  Electrolysis, however, produces zinc oxide at the anode and god 
knows what in solution.  Same, presumably, for cadmium.  Not the same as 
running water through it.

Keziah

----- Original Message ----- 
From: "David E. Smucker" <davesmucker at hotmail.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Saturday, February 23, 2008 9:02 AM
Subject: Re: [TheForge] Removing Zinc and Cadium


> Yes,  Galvanized water pipe is galvanized on both the inside and out. 
> Take a look at some.
>
> Dave
> ----- Original Message ----- 
> From: "Peter Hirst" <saltydog335 at aol.com>
> To: <GHS at execpc.com>; "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Friday, February 22, 2008 10:57 PM
> Subject: Re: [TheForge] Removing Zinc and Cadium
>
>
>> Galvanized on the inside?
>>
>> ;-]
>>
>> ----- Original Message ----- 
>> From: "GRAF" <adveniam at att.net>
>> To: "terry l. ridder" <terrylr at blauedonau.com>; "Sponsored by ABANA" 
>> <theforge at mailman.qth.net>
>> Sent: Friday, February 22, 2008 9:55 PM
>> Subject: Re: [TheForge] Removing Zinc and Cadium
>>
>>
>>> In the amounts and concentrations we would generate no problem.
>>> They still make and use Galvanized iron water pipe and you drink that!.
>>>
>>> Mike Graf
>>>
>>> terry l. ridder wrote:
>>>> hello;
>>>>
>>>> On Fri, 22 Feb 2008, Mitch Quade wrote:
>>>>
>>>>>
>>>>> A real easy way to remove Cadium and may
>>>>> be zinc is to put the screws in vinegar
>>>>> for several hours.
>>>>>
>>>>
>>>> yes, this does work. however, the cadmium and zinc
>>>> are now in solution with the vinegar. this is now
>>>> a liquid hazardous waste to dispose of.
>>>>
>>>> the removal of cadmium and/or zinc by electrolysis
>>>> would keep most of the cadmium and/or zinc as solids.
>>>>
>>> _______________________________________________
>>> Manage membership or unsubscribe at:
>>> http://mailman.qth.net/mailman/listinfo/theforge
>>> theforge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login:  blacksmithblacksmith at hotmail.com
>>> password:  anvil
>>> ___________
>>>
>>>
>>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
> 



More information about the TheForge mailing list