Electrolysis will remove the zinc in jiffy, and then proceed to oxidize
whatever is underneath it even jiffier. Take it from someone who had to use
a plated anode in a pinch one time.
Keziah.
----- Original Message -----
From: "terry l. ridder" <terrylr at blauedonau.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, February 22, 2008 9:56 AM
Subject: Re: [TheForge] DO NOT BURN OFF ZINC (GALVANIZED)
> hello bruce;
>
> do you know if there is a safe and reasonable method
> to remove zinc with electrolysis?
>
> On Fri, 22 Feb 2008, Bruce Freeman wrote:
>
>> If any of you are STILL tempted to BURN zinc plating off steel, READ
>> THIS: (shouting intentional!)
>>
>> http://www.anvilfire.com/iForge/tutor/safety3/index.htm
>>
>> What makes this death so very, very sad is that zinc can be pickled
>> off steel quickly, easily and with very little hazard.
>>
> <snip>
>>
>> Bruce
>> NJ
>>
>
> --
> terry l. ridder ><>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list