hello bruce;
do you know if there is a safe and reasonable method
to remove zinc with electrolysis?
On Fri, 22 Feb 2008, Bruce Freeman wrote:
> If any of you are STILL tempted to BURN zinc plating off steel, READ
> THIS: (shouting intentional!)
>
> http://www.anvilfire.com/iForge/tutor/safety3/index.htm
>
> What makes this death so very, very sad is that zinc can be pickled
> off steel quickly, easily and with very little hazard.
>
<snip>
>
> Bruce
> NJ
>
--