[TheForge] charcoal question

Jonathan Barnhart blakkpawss at yahoo.com
Tue Feb 19 11:24:45 EST 2008


Considering the Ice storm that we just went through in
my neck of the woods, it would probably be easy to
pick up a bunch of wood fot free and then process it
into fuel.  Even junk wood will make charcoal.  It
just doesn't burn as long or quite as hot.  But it you
have a lot of it, it might not make much differance.

--- Dan Scheid <Damales at pollybutte.net> wrote:

> Make it. It simple to do
> Take a good hard wood like oak burn it in a hole
> when the fire gets good and
> hot bury the fire. Wait until morning dig out the
> charcoal. If you like it
> then build a real retort.
> Dan Scheid
> 
> 
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf
> Of Bob Brashear
> Sent: Monday, February 18, 2008 8:22 PM
> To: The Forge
> Subject: [TheForge] charcoal question
> 
> I know not to use Kingsford or anything like its'
> ilk. What would you 
> guys recommend getting hold of? Just want to
> experiment some.
> 
> Thanks.
> 
> Bob Brashear
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> No virus found in this incoming message.
> Checked by AVG Free Edition. 
> Version: 7.5.516 / Virus Database: 269.20.7/1285 -
> Release Date: 2/18/2008
> 5:50 AM
>  
> 
> No virus found in this outgoing message.
> Checked by AVG Free Edition. 
> Version: 7.5.516 / Virus Database: 269.20.7/1285 -
> Release Date: 2/18/2008
> 5:50 AM
>  
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 



      ____________________________________________________________________________________
Be a better friend, newshound, and 
know-it-all with Yahoo! Mobile.  Try it now.  http://mobile.yahoo.com/;_ylt=Ahu06i62sR8HDtDypao8Wcj9tAcJ 



More information about the TheForge mailing list