I think that all you need is a reverse hardy hole.  Probably doesn't even need to hold the spike tight, just keep it reasonably vertical and centered.  

If you had a double ended  bar with the square hole on each end, you might be able to lock an indexing spike to your drill press table and be able to quickly drop your work into place without having to clamp/un-clamp it.
============================================================
From: ries <ries at riesniemi.com>
Date: Thu Feb 14, 11:16 AM
To: Sponsored by ABANA <theforge at mailman.qth.net>
Subject: Re: [TheForge] Drawer pulls

This would work- but me, I would use metal.
I cant imagine why.
I would take two blocks of steel, maybe 1" x 2" x 2", and make a  
spring swage handle for them, weld it together, then heat em up in the  
forge. When hot, put it in the power hammer with a spike.
Hit it hard.
Then, you put the spring swage in the vise. It holds a spike as if it  
was made for it.
Of course, you might have to grind a bit on the blocks to get exact  
orientation in the vise, but once that was done, it would work every  
time.
I always drill holes like this in my milling machine- it is so much  
more ridgid than a drill press, the vise alone weighs about what a  
cheapo harbor freight drill press does.
The holes come out straighter, I break fewer bits, and its quicker.

ries


On Feb 14, 2008, at 7:39 AM, Grant Marcoux wrote:

Ron:  to hold this RR spike head, why not make a conforming mould from
"Quick Crete" or other fast setting concrete product?  To do this,  
make a
ball of the material, press the head into it and allow to dry hard; just
make sure the base of the mould is kept flat enough to epoxy to a  
piece of
wood.  then you have a conforming rigid mould that can be glued to a  
small
square of plywood which can then be held on the drill press with a DP  
clamp.
Grant

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Ron Childers
Sent: Thursday, February 14, 2008 4:58 AM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] Drawer pulls


Mike,

A gentleman is building a log house and wants all the hardware made of
railroad spikes. My idea for the drawer pulls and cabinet knobs is to  
cut
about 1" from the head then drill and tap for 1/4" screws.

That part of the job is tedious and not very vain glorious, but we  
will have
to adapt a drill press vice to hold the head so the shank is perfectly
straight and exactly centered.  If it was only six or eight, I would
consider fullering and squaring with a monkey tool, then tapping for a  
1/4"
nut.

The door handles and knockers are a more interesting and creative part  
of
this undertaking, but the fastening aspect is similar.

If there is a better way, I'm open to suggestions.

Ron C


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________

No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.5.516 / Virus Database: 269.20.4/1276 - Release Date:  
2/13/2008
9:41 AM

No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.5.516 / Virus Database: 269.20.4/1276 - Release Date:  
2/13/2008
9:41 AM

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________



Ries Niemi
Industrial Artist
http://www.riesniemi.com/





_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________


============================================================




More information about the TheForge mailing list