On Mon, Dec 15, 2008 at 3:45 PM, Jerry Smith
<jerry_smith at anvilsandinkstudios.com> wrote:
> If you break a tap off, put the whole thing in the freezer. The broken
> tap will shrink away from what ever you have tapped. If you don't
> believe me, try it.
>
> Je