Some smiths around here use a flux that is a mixture of boric acid (roach 
kill) and iron oxide.  They get the iron oxide from the pottery suppliers. 
I don't understand the chemistry of what is happening at the melt 
temperatures.  This flux seems to work very well for them.

Dave
----- Original Message ----- 
From: "Peter Hirst" <saltydog335 at aol.com>
To: <mspencer at tallships.ca>; "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Monday, April 14, 2008 10:37 PM
Subject: Re: [TheForge] Re: New Discoveries: Ersatz EZ Weld


> Except band saw bits are steel.  Grinder bits are oxide.  I'm not sure 
> what good they do in flux.  In fact, i am wondering if the spec sheet I 
> saw on EZ weld could be correct.  Silica slag, sure.  But oxides?
>
>
>
> ----- Original Message ----- 
> From: "Mike Spencer" <mspencer at tallships.ca>
> To: <theforge at mailman.qth.net>
> Sent: Monday, April 14, 2008 10:10 PM
> Subject: [TheForge] Re: New Discoveries: Ersatz EZ Weld
>
>
>>
>>> So do I throw a bunch of scale or grinder dust in with the borax an
>>> steel shavings?
>>
>> If you collect the grinder dust (or band saw chips) with a magnet, you
>> can (mostly)  exclude non-ferrous bits, glass- and abrasive-dust
>> from the wheel, underbody roadgrime and other unwanted detritus.
>>
>> Or maybe that doesn't matter.
>>
>>
>> - Mike
>>
>> -- 
>> Michael Spencer                  Nova Scotia, Canada       .~.
>>                                                           /V\
>> mspencer at tallships.ca                                     /( )\
>> http://home.tallships.ca/mspencer/                        ^^-^^
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
> 



More information about the TheForge mailing list