Mon Apr 14 20:02:59 EDT 2008
Not nearly the volume. Real EZ Weld is 35-45% steel shavings. Even on days
we do what for us is a lot of cutting, we get maybe a tablespoon of
shavings. with the mill, I get that out of one pad in two minutes.
----- Original Message -----
From: "Franklin Police" <780 at mchsi.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Monday, April 14, 2008 7:31 PM
Subject: RE: [TheForge] New Discoveries: Ersatz EZ Weld
Why not go to the band saw and get the cuttings
Roger R Degner
The epoxy solvent series was so much fun I thought I'd contribute my own
discovery. I need a bunch of EZ Weld for an upcoming project, and seem to
recall it is just borax with iron filings. SO I have been pondering what
might be a cheap easy source of iron filings. Filing iron, as it turns out,
is not it.
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list