[TheForge] dies

Grant Marcoux gblacksmith at alamedanet.net
Sat Apr 12 15:37:37 EDT 2008


Kim:  S-7 is a rather high alloy material....you can heat treat it best if
you have a programmable kiln.  You may just want to send it out.

However, S-7 HT instructions are all over the web...just search "S-7 Heat
treating"

Grant

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of kim george
Sent: Saturday, April 12, 2008 7:54 AM
To: knife-list at kepler-eng.com; theforge at mailman.qth.net
Subject: [TheForge] dies


I have some s-7 that I am making into dies. What's the heat treat? or do I
have to send them out?

Kim George

       "Why for you burry me in cold,cold ground?" Taz





E-mail message checked by Spyware Doctor (5.5.0.212)
Database version: 5.09590
http://www.pctools.com/en/spyware-doctor/

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________

No virus found in this incoming message.
Checked by AVG.
Version: 7.5.519 / Virus Database: 269.22.12/1374 - Release Date: 4/11/2008
4:59 PM

No virus found in this outgoing message.
Checked by AVG.
Version: 7.5.519 / Virus Database: 269.22.13/1375 - Release Date: 4/12/2008
11:32 AM



More information about the TheForge mailing list