[TheForge] dies

kim george klgeorge at kent.edu
Fri Apr 4 12:00:12 EST 2008


I want to make a die to do ladder pattern. So what is the spacing and depth 
that I need for the die? I'll problem be working with a billet 5/8" thick 
or do I need it closer to the finish dimension? I thought I'd use H-13 or H-7.

Kim George

       "Why for you burry me in cold,cold ground?" Taz