[TheForge] ball peins
Mike Linn
bamablacksmith at comcast.net
Mon Sep 10 21:46:58 EDT 2007
Those who buy up ball peens to make striking tools will love this.
http://www.harborfreightusa.com/html/emails/37/RetailA/Images/13.gif
ok steel for the investment. Knock out the handle, forge the peen to
the desired shape, re-harden the working end and temper the face... re-handle
easy...