I am curious, how much baking soda should one use?
Rob
On Oct 21, 2007, at 07:43, Dan Scheid wrote:
You could use a battery charger. I have a 55 gal plastic drum with
water and
baking soda in it place your work in. Then place a chunk of Stainless
steel
in. Hook the negative lead to the work the positive to the SS. Set to 2
amps
come back in 2 days you will have a gray coat that cleans off easy
Dan Scheid
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Cindy and James
Sent: Sunday, October 21, 2007 6:31 AM
To: theforge at mailman.qth.net
Subject: [TheForge] Cleaning components
I have a bunch of component parts (small and a bunch of them 3-4 feet
long) for a project that need cleaning, deburring, etc. My current
method is to chuck them up in the vise, 1 by 1, wire brush, etc., etc.,
etc.
I got the idea from a conference to build a tumbler. Just dump all the
stuff in along with ball bearings for media and turn it on. Probably
overnight would do the trick.
Question for the group... Have any of you used/built a tumbler for this
process? If so, what size was it? How did you power it? How well did
it work and was it worth the effort? What approx. RPM did you run it.
My thoughts on building one is to buy a piece of 24 to 30 inch diameter
pipe, weld plate to the ends, weld trailer or auto axle stubs in the
center of the plate and use the running gear portion (bearings, etc), to
support the whole thing welded to a framework of some sort. Put a
pulley on it and a motor and away you go.
Another idea, a little more challenging (for me) would be to mount it on
2 auto differentials with wheels and tires, mounted parallel, they would
support the rig and permit turning, either by powering the gearbox or
with a pulley direct to the tumbler.
Right now, I like method 1 better. Seems simpler, quicker, easier,
smaller footprint.
My scrap yard has a 16 or 20 foot stick of 20" for about $10 a foot.
I'd use about 5 or 6 feet, keep the rest for BBQ smokers/pits. They
also have a 5' piece of 29" for about $14/ft. Both are around 5/8 to
3/4 wall pipe, I didn't measure, just looked. Either one would be
pretty heavy and require a pretty good motor to start it going.
Probably pretty noisy.
I've thought about getting an old clothes dryer to use for small stuff
till I get this thing built. It would also tell me if it would work,
and how well.
Ideas, comments?
James Allcorn
Bois D'Arc Forge Blacksmith Shop
Paris, TX
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.5.488 / Virus Database: 269.15.3/1081 - Release Date:
10/19/2007
5:41 PM
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.5.488 / Virus Database: 269.15.3/1081 - Release Date:
10/19/2007
5:41 PM
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list