Mark,
I run my 30 pounder with a 6HP with a total of 120
gallon of air tanks. It's not so much the compressor
as it's the air volume you have.
Jerry
--- "Mark A. Pesetsky" <pesetsky at Princeton.EDU> wrote:
> How many CFM's are you guys pulling on say a #40
> hammer? Need to start
> looking for a compressor soon.
>
> Thanks
> Mark
>