--- Kathy <keporter at comcast.net> wrote:

> For use on ceramic blanket, dab Rigidizer (colloidal
> silica) on with a cheap
> paint brush, allowing it to sink in to a depth of
> between 1/4” and 1/2”, in
> order to create a semi rigid under layer—not given
> to shrinking due to heat
> exposure—on the inner face (hot face side) of a
> ceramic blanket; after heat
> curing, paint a coating of Plistex (ordered from
> Larry Zoeller) in order to
> create a very tough finish layer; after heat curing
> the Plistex, paint on a
> final coating of water separated ITC-100 or a
> combination of water separated
> (colloidal) #200 mesh zirconium and a dab of water
> separated clay (as a binder).
> The above combination gives the toughest, and most
> infrared reflective finish
> presently possible for hobby use ceramic refractory
> blanket insulation.
> 
>  
> 
> However, it is silly to use ceramic blanket unless
> the forge is either going to
> be transported a lot, or needs to cool down at
> maximum speed (twenty minuets to
> less than 140° F from yellow heat); as in the case
> of a home hobbyist worried
> over safety issues and with limited time (husbands
> and fathers). Otherwise, an
> extra five minuets heat up period (but up to four
> hours cool down time) will
> allow the use of an insulating refractory like
> Kastolite #3000. A good quality
> insulating refractory will hold up far better than
> the toughest and most
> carefully prepared ceramic blanket insulation on
> shop forges (still
> transportable, but heavier).
> 
> Mikey    
> 
>  
> 
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net]
> On Behalf Of Ron Childers
> Sent: Thursday, May 24, 2007 7:33 AM
> To: 'Sponsored by ABANA'
> Subject: RE: [TheForge] Mineral Wool & satinite vs
> IT?C-100, etc
> 
>  
> 
> Kaowool seems to work ok; I guess Plistex or ITC-100
> could be applied over
> 
> satinite if it would be of appreciable benefit...?
> 
>  
> 
> Ron C
> 
>  
> 
> -----Original Message-----
> 
> From: theforge-bounces at mailman.qth.net
> 
> [mailto:theforge-bounces at mailman.qth.net] On Behalf
> Of Steven Smith
> 
> Sent: Thursday, May 24, 2007 10:10 AM
> 
> To: Sponsored by ABANA
> 
> Subject: Re: [TheForge] Mineral Wool
> 
>  
> 
> Both Kaowool and Durablanket are brand names. Within
> each brand name are 
> 
> different products designed to work at different
> temperatures. You will 
> 
> be unhappy if you get an inexpensive, low
> temperature wool. I use 
> 
> Durablanket "S".
> 
>  
> 
> I agree with Bruce's recommendation of 2" thick, 8
> pounds per cubic foot 
> 
> density. The denser stuff lasts better against
> mechanical damage. You 
> 
> also should put a seal coat on the inside of your
> forge. You make up a 
> 
> sort of mud and paint it on. I use Satanite. More
> expensive options that 
> 
> reflect IR and improve the efficiency of your forge
> include ITC100.
> 
>  
> 
> I do wish someone would measure before and after
> with ITC100. So far, 
> 
> all I've heard is anecdotal "it was hotter".
> 
>  
> 
> Steve
> 
>  
> 
> Jerry Smith wrote:
> 
> > Folks,
> 
> > 
> 
> > I need a number or a name or something for model
> or
> 
> > brand of mineral wool, I need to buy some mineral
> wool
> 
> > for rebuilding my forge and to build a new furnace
> for
> 
> > melting glass.
> 
> > 
> 
> > I am using Frosty's design for the burner, it
> works
> 
> > great for me.
> 
> > 
> 
> > 
> 
> > Thanks,
> 
> > 
> 
> > Jerry
> 
> > 
> 
> > _______________________________________________
> 
> > Manage membership or unsubscribe at:
> 
> > http://mailman.qth.net/mailman/listinfo/theforge
> 
> > theforge mail list group photo site is
> 
> > http://www.photoaccess.com
> 
> > Login:  blacksmithblacksmith at hotmail.com
> 
> > password:  anvil
> 
> > ___________
> 
> > 
> 
> > 
> 
> > 
> 
> >   
> 
>  
> 
> _______________________________________________
> 
> Manage membership or unsubscribe at:
> 
> http://mailman.qth.net/mailman/listinfo/theforge
> 
> theforge mail list group photo site is
> 
> http://www.photoaccess.com
> 
> Login:  blacksmithblacksmith at hotmail.com
> 
> password:  anvil
> 
> ___________
> 
> 
=== message truncated ===



More information about the TheForge mailing list