[TheForge] oops...Kaowool

Jerry Smith jerry_smith at anvilsandinkstudios.com
Thu May 24 11:11:26 EDT 2007


I live in Eastern Ohio, near Wheeling West Virginia

Jerry

--- Andy Gladish <gladish at cablerocket.com> wrote:

> 
> Jerry, I don't know what part of the country you
> live in, but here by the
> seacoast I find Kaowool in the local marine supply
> place. They probably use
> it for insulating boat exhausts.
> 
> Andy Gladish
> 
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 



More information about the TheForge mailing list