I prefer cerachem and cerachrome with satanite as a protector for the blanket

http://www.thermalceramics.com/upload/pdf/514-205.pdf



mike



At 09:55 PM 5/23/2007, you wrote:
>I don't have the information at my fingertips and
>would have to do a search to find it.  Kaowool is one
>brand.
>
>I suggest you get the 2" thick material, 8#/cu.ft.
>You can  make do with two layers of the 1" material,
>but the density is important.
>