Cool...thanks...If using straight C02 there is an adaptor that came
w/the kit.

Thanks Again
Mark 



In that case, if you aren't needing maximum penetration, I would go with
the 75%/25% mix.  However if you want deeper penetration and a hotter
weld, go with straight CO2.  There are a few other hotter mixes, but
those are the common cheap options.