[TheForge] MIG Welders

Jerry Frost frosty at customcpu.com
Tue May 22 01:18:33 EDT 2007


I have a Hobart 120 Handler that's about 15+ years old 
and it's been rock steady. I can't say anything about 
them since Miller bought them out though.

Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks

Meadow Lakes, AK.

http://www.artmetalradio.com/

From: "The Millers" <debmiller at fuse.net>


>I have two Lincoln MIGs. An old WeldPak 100, 110v and 
>a WeldPak 150  which 220v.
> I have used them regularly for 10 years with not one 
> lick of trouble.  Consumables are readily available 
> and pretty generic.
>
> ITW owns, Miller and Hobart and I believe Hobart to 
> be ITW's entry  level  machines, nowadays. If you can 
> get your hands on an old Hobart  Handler 120 it would 
> serve you well, too.
>
> Ray Miller
> Cincinnati