[TheForge] acid
PlumDon at aol.com
PlumDon at aol.com
Sun May 13 07:27:57 EDT 2007
In a message dated 5/13/2007 6:21:51 AM Eastern Daylight Time, PlumDon
writes:
In a message dated 5/12/2007 11:10:21 PM Eastern Daylight Time,
dan at irontreeworks.com writes:
1 gallon of regent grade Sulfuric Acid
Can anyone recommend a use for the the others or different uses than the
ones I already mentioned?
------------------------------------------------------------------------------
-------------------------
I assume that is about 65%. Excellent for passivating stainless steel. After
forging a 5-10 minute bath will remove all the surface iron and you will
once again have a chromium stainless steel surface.