[TheForge] OT sort of Powder Coating
ries
ries at riesniemi.com
Sun Mar 18 18:27:52 EST 2007
I am not sure 250 is hot enough.
I seem to remember a range of 300 to 500 degrees, depending on the
size of work and the type of powder.
One person you might want to talk to is Jack Brubaker-
http://www.jackbrubaker.com/index-2.html
He built his own powdercoating setup to do his candlesticks with- It
seems to me he uses a homemade propane fired oven.
From out here, on the West Coast, Indiana looks right next to Ohio-
Why he's practically next door to you.
Of course, I have to drive for two solid days just to get to San
Francisco, so maybe my idea of distance is different than yours.
ries
On Mar 18, 2007, at 3:29 PM, Jerry Smith wrote:
Ries,
I haven't gotten the gun and the materials yet. What I
have is bead/grit blasting booth(HF), a good
compressor, a 18 inch bt 18 inch bt 16 inch oven and a
smaller one that in 12 x 12 x 12, both capable of
reaching 250 degree C. Spray booths are easy to build
and I have several shop vacs that can be used.
I want to look at what people have for the spray
process.
Thanks,
Jerry
--- ries <ries@
> I have never done it myself, but I have been paying
> people to do it
> since about 1988.
> I have sent several powder coaters kids to college.
> We used to do production pieces like candlesticks
> and soap dishes,
> where we might do 200 at a time, or a dozen chairs,
> or sculptural
> elements as big as 20 feet long.
>
> Things I learned:
>
> Sandblasting is good. Not essential, but it sure
> doesnt hurt,
> especially on hot rolled. We did some production
> pieces for a few
> years made from rebar (chairs, small tables, and so
> on) and it all
> needed to be blasted.
>
> Cold rolled can be run without blasting, but it
> needs to be really
> clean.
> Wiping down with alchohol or a solvent will work.
>
> All the pros use phosphate pre-dip systems- The vast
> majority of my
> stuff had this done to it- my last guy had a 5 tank
> system- a mild
> etch, then rinse, then phosphate, then rinse again-
> cant remember
> what the last one was.
> Anyway, the point is, the stuff needs to be REALLY
> clean.
>
> For clearcoated stuff, we would fine sand or wire
> brush it right
> before blasting, then handle with white cotton
> gloves.
>
> Aluminum, especially castings, but not only, needs
> to be preheated at
> 300 to 400 degrees for a good 20 minutes first-
> otherwise, moisture
> always shows up and makes bubbles and pinholes.
>
> Good powder is expensive- I mostly used Tiger
> Drylac, Cardinal, and
> the major brands just for stuff like Black Wrinkle
> or plain colors-
> for the fancy stuff, the best, most distinctive
> colors and textures
> come from Prismatic-
> http://www.nicindustries.com/prismatic_powders.php
>
> they cost a lot more per pound than places like
> Eastwood, but they
> are really worth it.
>
> I recommend using textures or wrinkles in most
> cases- they wear much
> better, hide scratches and handling marks.
> Gloss finishes are the worst, in terms of fragility-
> Powder is not as
> tough as something like laquer, its pretty easy to
> ruin a gloss finish.
>
> There is no touchup with powder- if you screw up,
> you need to remove
> it, and start over- and it aint easy to get it off.
> The pro shops I
> dealt with use a 2000 degree burnout oven- which,
> since they did
> things like furniture, was big- it had a little
> railroad track going
> in it for a dolly about 4 feet square. It does not
> want to sandblast
> off without being burned first- and the fumes are
> nasty. You can, in
> a pinch, use a rosebud, but it will probably shorten
> your life by a
> few months every time.
> My old industrial sandblaster in LA, who had
> something like 3
> compressors, each 200hp, and air hoses as big as
> your arm, flat out
> refused to sandblast powdercoating, as nobody would
> ever want to pay
> what it really cost, as it took SO long.
>
> Best type of oven is one you can roll a cart into-
> then you can hang
> the parts, shoot em, and roll it right in.
> I like to deal with guys who have 20' x 10' x 10'
> ovens, as I tend to
> do big stuff- and even with chairs, you cant
> economically do em if
> you can only do one part every half hour, so they
> would rack up a
> whole dozen or two at a time.
>
> For itty bitty stuff, yeah, you could use an old
> home oven- if time
> is not a concern. But if you get into doing it much,
> you are going to
> want a bigger oven.
>
> The $200 guns work. Just like a $500 Harbor Freight
> lathe will work.
> But just like a real machinist will want a $20,000
> used Monarch, a
> real powder coater will spend $5000 and up on a
> decent pro gun.
> Partly its long life, ease of use, and volume, but
> the real guns do a
> better job as well.
> So dont expect to get the greatest results from
> those little guns.
> Clean, dry air, of course, is a must.
>
> If you are doing the occasional, jewelry sized
> object, and dont mind
> fussing, then you may have success with the cheapo
> route.
>
> If you are doing much for resale, and any kind of
> volume, I think you
> will quickly find its worth it to use a pro shop.
> The average guy I dealt with ( 5 different big shops
> over the last 25
> years- In LA, Ventura, and couple up here in
> Washington)
> had well over $100,000 invested in equipment.
>
> Ries
>
>
>
>
>
>
> On Mar 18, 2007, at 11:28 AM, Jerry Smith wrote:
>
> Folks,
>
> Do we have any one out there who does powder
> coating?
> I wan to learn how to do it, and also how to avoid
> the
> mistakes.
>
> I don't have the gun or the basic kit, but I do have
> a
> compressor and a good size oven.
>
> Jerry
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
> Ries Niemi
> Industrial Artist
> http://www.riesniemi.com/
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
Ries Niemi
Industrial Artist
http://www.riesniemi.com/
More information about the TheForge
mailing list