[TheForge] TIG Welder

Woolley wjec at verizon.net
Mon Mar 5 21:07:35 EST 2007


Who knows?  Talk to people using the machines.  Try out the machine at the 
dealer.


----- Original Message ----- 
From: "Ron Swisher" <rwswisher at verizon.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Monday, March 05, 2007 9:03 PM
Subject: Re: [TheForge] TIG Welder


> Yes, 250-325 amps is what Miller says one needs to lap weld 1/4" mild or 
> stainless steel with a TIG.  Why would Miller say this when it is 
> obviously false?
>