[TheForge] TIG Welder
Woolley
wjec at verizon.net
Mon Mar 5 20:37:05 EST 2007
> For a 1/4" lap weld the settings are 250 - 325 amps.
For a 1/4" lap weld on what? If you want to put a 1/4" pass on say 2 pieces
of 1/4" plate, 250 amps would probably burn a hole in it with stick. You
might put a 1/4" weld with one pass with say jet rod but I'm guessing the
amps might approach 160-175 max. There are many ways (processes, materials
etc) to put a 1/4" weld on whatever thickness steel but none of them involve
250-325 amps.
Bill Woolley
More information about the TheForge